Pojedinosti proizvoda
Osnovni podaci
Materijal: Polivinil Klorid/PVC
Korištenje: General plastike
Boja: žuta
Porijeklo: Kina
HS kod: 1518000000
Opis proizvoda
Epoxidized soja oil(ESO)
Svojstva: Svjetlo žuta gusta masnu tekućinu u normalnu temperaturu, molekularne formule C57H106O10, molekularna težina 1000, pour point - 3C, vrenja 150 (0.5kpa), Viskoznost 325mpa.s, loma indeks 1.472(25C), topivost u vodi< 0.01%(25c).="" it="" is="" one="" kind="" of="" chemical="" auxiliary="" for="" food="" packing,="" it="" can="" be="" used="" in="" all="" pvc="" materials,="" ,="" including="" food="" packing,="" medicinal="" appliance,="" film,="" sheet,="" board,="" sealing="" stripe,="" artificial="" leather,="" plastic="" wall="" paper,="" cable,="" daily="" plastic="" products,="" special="" ink,="" paint,="" coating,="" chemical="" rubber="" and="" liquid="">
Doziranje: To možete raditi s Poliester plastifikator smanjiti migraciju Poliester plastifikator ili rad s metalnih topline stabilizator. Kompatibilnost je slična dop-a i njegov politicizing učinak je bolji nego dop-a, čime možete poboljšati kvalitetu i niže troškove. Za meke proizvode, doza je 5 do 10 porcija. U posebno stanje, doza je 10 do 30 porcija. Nego može biti upotrijebljen kao zamjena plastifikator, stabilizator i lubrikant djelomično.
Pakovanje: 200kg bubnjevi, 1000L IBC bubnjevi, Flexitanks